A full-size fracture of tight sandstone induced by water, N2 and CO2



Data

Initial_1_00900.tiff
3.9 MB

Initial_1_00901.tiff
3.9 MB

Initial_1_00902.tiff
3.9 MB

Initial_1_00903.tiff
3.9 MB

Initial_1_00904.tiff
3.9 MB

Initial_1_00905.tiff
3.9 MB

Initial_1_00906.tiff
3.9 MB

Initial_1_00907.tiff
3.9 MB

Initial_1_00908.tiff
3.9 MB

Initial_1_00909.tiff
3.9 MB

Initial_1_00910.tiff
3.9 MB

Initial_1_00911.tiff
3.9 MB

Initial_1_00912.tiff
3.9 MB

Initial_1_00913.tiff
3.9 MB

Initial_1_00914.tiff
3.9 MB

Initial_1_00915.tiff
3.9 MB

Initial_1_00916.tiff
3.9 MB

Initial_1_00917.tiff
3.9 MB

Initial_1_00918.tiff
3.9 MB

Initial_1_00919.tiff
3.9 MB